| Standard | GOST 4784-97, GOST 21631-76 | GOST 4784-97, GOST 21631-76 |
| Similar Grades (Analogues) | EN AW-2017A (Europe), 2017 (USA), AlCu4MgSi | EN AW-2024 (Europe), 2024 (USA), AlCu4Mg1 |
| Alloy Type | Wrought, medium-strength, general purpose | Wrought, high-strength, aircraft-grade |
| Chemical Composition | Al: baseCu: 1.2–1.8%Mg: 0.4–0.8%Mn: 0.4–1.0%Si: ≤0.5%Fe: ≤0.7%Zn: ≤0.3%Ti: ≤0.15%Cr: ≤0.1% | Al: baseCu: 3.8–4.9%Mg: 1.2–1.8%Mn: 0.3–0.9%Si: ≤0.5%Fe: ≤0.5%Zn: ≤0.25%Ti: ≤0.15%Cr: ≤0.1% |
| Delivery Condition | N = Normalized (annealed) | AT = Solution heat-treated and naturally aged |
| Mechanical Properties | - Tensile strength: 295–390 MPa- Yield strength: 180–250 MPa- Elongation: 10–18%- Hardness (HB): ~80–100 | - Tensile strength: 410–470 MPa- Yield strength: 250–325 MPa- Elongation: 10–15%- Hardness (HB): ~120–140 |
| Technological Properties | - Good machinability- Good weldability- Good corrosion resistance- Easily extruded and rolled | - Good machinability- Poor weldability (prone to hot cracking)- High strength-to-weight ratio- Good fatigue resistance- Moderate corrosion resistance (often clad for protection) |
| Applications | - General engineering- Construction- Automotive parts- Rivets, fasteners | - Aircraft structures- Aerospace- High-load parts- Automotive, military applications |
| Heat Treatment | Annealed (N): soft, ductile | Solution heat-treated + natural aging (AT): high strength |
| Advantages | - Easy to process- Good formability- Versatile | - High strength- Good fatigue resistance- Widely used in aerospace |
| Disadvantages | - Lower strength than D16AT- Not for high-load applications | - Poor weldability- Susceptible to stress corrosion- Needs protection against corrosion |
| Corrosion Resistance | Good | Moderate (often clad with pure Al for protection) |