| Standards | GOST 1050-88 (Russian standard for quality carbon structural steel) | GOST 4543-71 (Russian standard for alloyed structural steel) |
| Similar Grades (Analogues) | - AISI 1020 (USA)- S20C (Japan)- C22 (Germany, DIN) | - 18CrMnTi (China)- 20MnCr5 (Germany, DIN)- AISI 5120 (USA) |
| Chemical Composition | - C: 0.17–0.24%- Si: 0.17–0.37%- Mn: 0.35–0.65%- P: ≤0.035%- S: ≤0.035%- Ni: ≤0.30%- Cr: ≤0.25%- Cu: ≤0.30% | - C: 0.17–0.23%- Si: 0.17–0.37%- Mn: 0.80–1.10%- Cr: 1.00–1.30%- Ti: 0.04–0.10%- P: ≤0.035%- S: ≤0.035%- Ni: ≤0.30% |
| Mechanical Properties | (After normalization at 880–900°C)- Tensile strength: 410–550 MPa- Yield strength: ≥245 MPa- Elongation: ≥25%- Hardness (HB): 121–156 | (After quenching and tempering)- Tensile strength: 900–1100 MPa- Yield strength: ≥700 MPa- Elongation: ≥10%- Hardness (HB): 229–269 |
| Technological Properties | - Good weldability (no preheating required)- Excellent machinability- Suitable for cold forming- Limited hardenability (low carbon content) | - Moderate weldability (preheating and post-weld heat treatment recommended)- Good machinability after annealing- High hardenability due to alloying elements (Cr, Mn, Ti)- Suitable for surface hardening (carburizing, nitriding) |
| Applications | - Used for low-stress parts (bolts, screws, shafts, bushings)- Suitable for parts requiring good ductility and toughness- Commonly used in general engineering | - Used for high-strength, wear-resistant parts (gears, shafts, couplings)- Suitable for parts requiring surface hardening and high core strength- Common in automotive and machinery industries |
| Heat Treatment | - Normalization: 880–900°C- Annealing: 860–880°C- Carburizing possible but not common due to low hardenability | - Quenching: 860–880°C (oil)- Tempering: 180–200°C- Carburizing: 900–950°C- Suitable for nitriding and induction hardening |
| Advantages | - Low cost- Easy to process (welding, machining, forming)- Good ductility and toughness | - High strength and wear resistance- Excellent hardenability- Suitable for heavy-duty applications |
| Disadvantages | - Low strength and wear resistance- Not suitable for high-stress or high-wear applications | - Higher cost due to alloying elements- More complex processing (welding, heat treatment) |