Explaining S-N curves and endurance limits
S-N curves plot stress amplitude versus number of cycles to failure, showing that steel exhibits a fatigue (endurance) limit—a stress below which it can resist infinite cycles—while aluminum lacks this due to its microstructure allowing continuous slip and crack initiation. This difference arises from steel's BCC structure with strain aging and interstitials restricting dislocation motion at low stresses, versus aluminum's FCC structure with easier dislocation movement and more environmental sensitivity, meaning aluminum eventually fails even at low stress amplitudes.
If you take a batch of specimens and subject them to a constant, fully‑reversed stress and simply count how many cycles it takes before a fatigue crack runs through them, you can plot the result as stress amplitude versus cycles to failure. That plot is what is usually called an (S)–(N) curve. At high stress amplitudes you get rapid failure; as the stress is lowered the number of cycles increases by orders of magnitude. On a semi‑log or log–log plot most metals produce a family of falling curves.
For many plain carbon and low‑alloy steels those curves have a very pronounced “knee” at around 10^6–10^7 cycles and then flatten out. Below a certain alternating stress the data asymptote to a horizontal line and specimens will survive 10^7, 10^8… cycles without cracking. That horizontal asymptote is what is meant by the endurance or fatigue limit.
Two important points are worth noting about that:
-
The “never fails” is an idealisation. The limit is determined statistically, and corrosion, mean stresses, large stress concentrators etc. will bring the effective limit down. Modern high‑strength steels and many other alloys don’t show a perfectly horizontal region at all.
-
The existence of a limit is tied to the underlying deformation mechanisms. In ferritic BCC steels at room temperature dislocation motion is comparatively difficult: interstitial carbon and nitrogen atoms pin dislocations, and dynamic strain ageing causes a significant increase in the stress required to move them. At very low stress amplitudes any small cracks that do form tend to arrest because there isn’t enough cyclic plasticity to sustain a growing crack.
Aluminium alloys, by contrast, are face‑centred cubic with a low Peierls barrier. Dislocations glide easily at ambient temperatures and there is no comparable strain‑ageing effect to lock them. Oxide films and second–phase particles provide ready sites for persistent slip bands. As a result the S–N curves for aluminium and most other non‑ferrous alloys simply continue to slope downwards: even a very small alternating stress will produce enough cyclic slip over a sufficient number of cycles for a crack to initiate and propagate.
Design practice reflects this difference. For steels it is common to design for “infinite life” below the endurance limit; for aluminium and similar alloys a finite life is assumed at any non‑zero alternating stress.