Designing a formulation for polybutadiene (BR) as an oxygen scavenger involves several considerations to ensure the resulting film effectively scavenges oxygen and maintains desirable physical properties. Here’s a step-by-step guide to creating such a formulation:
1. Selection of Polybutadiene (BR)
Choose a suitable grade of polybutadiene. Cis-1,4-polybutadiene is commonly used due to its good mechanical properties and flexibility.
2. Oxygen Scavenger Additives
Incorporate oxygen scavengers into the BR matrix. Common oxygen scavengers include:
- Iron-based scavengers: Iron powder or iron-based compounds.
- Ascorbic acid: Often used in food packaging.
- Enzymes: Certain enzymes can scavenge oxygen.
3. Antioxidants
Add antioxidants to stabilize the polybutadiene and prevent degradation during processing and use. Common antioxidants include:
- Phenolic antioxidants (e.g., Irganox 1010)
- Phosphites (e.g., Irgafos 168)
4. Plasticizers (Optional)
If flexibility is required, add plasticizers. Common plasticizers for polybutadiene include:
- Dioctyl phthalate (DOP)
- Dioctyl adipate (DOA)
5. Processing Aids
Incorporate processing aids to improve the processability of the formulation. Examples include:
- Stearic acid
- Zinc stearate
6. Fillers (Optional)
Fillers can be added to modify the mechanical properties or reduce cost. Common fillers include:
Example Formulation
Here’s an example formulation for an oxygen scavenging BR film:
Ingredients:
- Polybutadiene (BR): 100 parts by weight
- Oxygen Scavenger:
- Iron powder: 5-10 parts by weight
- Antioxidant:
- Irganox 1010: 1 part by weight
- Plasticizer (if needed):
- DOP: 5-10 parts by weight
- Processing Aid:
- Stearic acid: 1 part by weight
- Filler (optional):
- Calcium carbonate: 5-10 parts by weight
Processing Steps
- Mixing:
- Dry blend the polybutadiene with the iron powder, antioxidant, plasticizer (if used), processing aid, and filler (if used).
- Melt Compounding:
- Use a Banbury mixer or twin-screw extruder to melt compound the ingredients. Ensure thorough mixing to distribute the oxygen scavenger uniformly.
- Film Formation:
- Extrude the compounded material into a film using a flat film die.
- Cool the film on a chill roll and wind it up.
Testing
- Oxygen Scavenging Efficiency: Test the film’s oxygen scavenging capacity using an oxygen transmission rate (OTR) tester.
- Mechanical Properties: Evaluate tensile strength, elongation at break, and flexibility.
- Thermal Stability: Assess thermal stability using TGA (Thermogravimetric Analysis).
Applications
- Food packaging
- Pharmaceutical packaging
- Any application requiring oxygen barrier properties
By carefully selecting and combining these ingredients, you can create an effective oxygen scavenging polybutadiene film.