Excellent questions! You've identified some key implementation details.
Tensor vs Scalar in the PDE
In the PDE ε̄ᵖ - l²∇²ε̄ᵖ = εᵖ:
- εᵖ is typically a scalar - the equivalent plastic strain (like von Mises equivalent strain)
- ε̄ᵖ is also a scalar - the nonlocal equivalent plastic strain
The full plastic strain tensor ε̇ᵖ (which is indeed a tensor with 6 components in 3D) gets converted to the scalar εᵖ through:
εᵖ = ∫ √(2/3 ε̇ᵖᵈᵉᵛ : ε̇ᵖᵈᵉᵛ) dt
So the flow rule gives you the full tensor, but the gradient regularization typically acts on the scalar equivalent measure.
Flow Rule Confirmation
Yes, ε̇ᵖ in the flow rule is definitely a tensor (rank-2, with 6 independent components in 3D). The flow rule:
ε̇ᵖ = λ̇ ∂f/∂σ
gives you the full plastic strain rate tensor at each point.
Staggered Formulation - Great Idea!
Absolutely! A staggered approach is very common and much more practical:
Staggered Algorithm:
- At time step n+1, use ε̄ᵖⁿ (from previous step) in your J2 plasticity routine
- Solve mechanics: get new εᵖⁿ⁺¹
- Solve gradient PDE: ε̄ᵖⁿ⁺¹ - l²∇²ε̄ᵖⁿ⁺¹ = εᵖⁿ⁺¹
- Repeat
Advantages:
- Much easier to implement in existing code
- No need to modify global stiffness matrix structure
- Can be added as a post-processing step after each increment
Disadvantages:
- May need smaller time steps for stability
- Slight lag in nonlocal effects
This staggered approach would actually let you keep your integration point structure largely intact - you'd just need to add the gradient PDE solve as a separate step between increments.
Would you like me to elaborate on how to implement the gradient PDE solve efficiently?