The gate leakage current in a MOS capacitor arises from several mechanisms, each modeled differently based on oxide thickness, electric field, temperature, and defects. Below is a structured summary of the primary models:
1. Direct Tunneling (Band-to-Band Tunneling)
Conditions: Very thin oxides (( t_{\text{ox}} \lesssim 1 , \text{nm} )) and high electric fields.
Mechanism: Electrons tunnel directly through the oxide barrier due to quantum mechanical effects.
Model:
[
I \propto \exp\left(-\frac{\alpha}{t_{\text{ox}}}\right) \cdot \exp\left(-\frac{\beta}{E_{\text{ox}} \cdot t_{\text{ox}}}\right),
]
where ( E_{\text{ox}} = \frac{V_g}{t_{\text{ox}}} ), and (\alpha, \beta) are material-dependent constants.
Key Factor: Exponential dependence on oxide thickness and field.
2. Fowler-Nordheim Tunneling (Field Emission)
Conditions: High electric fields (( E_{\text{ox}} \gtrsim 3 , \text{MV/cm} )), typically in thinner oxides (( t_{\text{ox}} \lesssim 2 , \text{nm} )).
Mechanism: Electrons tunnel through the oxide barrier under extreme fields.
Model:
[
I = A \cdot \left(\frac{E_{\text{ox}}}{E_0}\right)^2 \cdot \exp\left(-\frac{B}{E_{\text{ox}}}\right),
]
where ( A ) and ( B ) are constants dependent on oxide material.
Key Factor: Quadratic dependence on ( E_{\text{ox}} ) and exponential decay with ( 1/E_{\text{ox}} ).
3. Thermal Emission (Schottky Emission)
Conditions: Moderate electric fields and elevated temperatures.
Mechanism: Electrons thermally excite over the oxide barrier.
Model:
[
I \propto \exp\left(-\frac{q\Phi}{kT}\right) \cdot \exp\left(\frac{qV_g}{kT}\right),
]
where ( \Phi ) is the effective barrier height.
Key Factor: Strong temperature dependence and exponential voltage dependence.
4. Interface Trap-Assisted Tunneling
Conditions: Presence of interface traps (density ( N_{\text{ss}} )) at the oxide-semiconductor interface.
Mechanism: Traps lower the effective barrier height, enabling leakage.
Model:
[
I \propto N_{\text{ss}} \cdot \exp\left(-\frac{E_{\text{t}}}{kT}\right) \cdot \left[ \exp\left(-\frac{q(V_g - \chi)}{kT}\right) - 1 \right],
]
where ( E_{\text{t}} ) is the trap energy level and ( \chi ) is the oxide-semiconductor work function difference.
Key Factor: Relies on trap density and energy distribution.
5. Bulk Defects in Oxide
Conditions: Oxide defects (e.g., oxygen vacancies) acting as conductive paths.
Mechanism: Defects create localized states that enable leakage.
Model:
[
I \propto N_{\text{defect}} \cdot \exp\left(-\frac{E_{\text{a}}}{kT}\right),
]
where ( N_{\text{defect}} ) is defect density and ( E_{\text{a}} ) is activation energy.
Key Factor: Activation energy and defect density dominate the leakage.
Moderate Voltage/Thick Oxide: Thermal emission transitions to tunneling.
High Voltage/Thin Oxide: Fowler-Nordheim or direct tunneling dominate.
Defects/Interface Traps: Contribute at all voltages but become significant in defective oxides.
These models collectively explain gate leakage, with the dominant mechanism depending on device parameters like ( V_g ), ( t_{\text{ox}} ), and oxide quality.