Please correct: Highlights of Activity/Results: 1) Cropped out and replated the bottom…
- User
Please correct: Highlights of Activity/Results:
- Cropped out and replated the bottom shell to repair the crack at FR. 27 port.
- Cropped out the bottom shelf inside the hull to access the back gouging.
- Refitted the closing plate after the back gouging and welding. Installed flat bar and follow the 3 way connection
- Conducted DPT and Vacuum test for acceptance.
- Assistant
Here’s a corrected and refined version of your text:
Highlights of Activities/Results:
- Cropped out and replated the bottom shell to repair the crack at FR. 27 port.
- Cropped out the bottom shelf inside the hull to access the back gouging.
- Refitted the closing plate after the back gouging and welding, and installed a flat bar to follow the three-way connection.
- Conducted Dye Penetrant Testing (DPT) and vacuum tests for acceptance.
- User
please correct: Highlights of Activity/Results:
- Cropped out and replate he bottom shell to repair the crack at Fr. 8-9 Port.
- Conducted dye penetration test and vacuum test after weldout.
- Conducted final inspection with the QA inspector and BV surveyor for acceptance.
- Assistant
Here’s a corrected and polished version of your text:
Highlights of Activities/Results:
- Cropped out and replated the bottom shell to repair the crack at FR. 8-9 port.
- Conducted a dye penetration test and vacuum test after welding.
- Conducted a final inspection with the QA inspector and BV surveyor for acceptance.
- User
Please correct: Highlights of Activity/Results:
- Completed surface preparation by buffing and removing all weld spatter.
- Applied primer and topcoats for anti-corrosion and antifouling.
- Assistant
Here’s a corrected and refined version of your text:
Highlights of Activities/Results:
- Completed surface preparation by buffing and removing all weld spatter.
- Applied primer and topcoats for anti-corrosion and antifouling protection.