A tank which operates under a stress of 620 MPa is known to contain edge cracks that grow at a rate of 5 μm month ⁄ . The fracture toughness of material from which the tank made is 48 MPa√𝑚. The Geometry factor (Y) of the specimen is 1. A proof-test for the duration of the tank is scheduled. Calculate the minimum stress (in MPa) that should be used in the proof-test if it is desired that the tank should operate safely for one year.
Assistant
To solve this problem, we need to ensure that the tank will operate safely for one year without the crack reaching a critical size that would lead to failure under the operating stress of 620 MPa. We also need to determine the proof-test stress that will ensure any crack that would reach critical size during operation will fail during the proof-test, thus preventing catastrophic failure during service.
Step 1: Calculate the critical crack size under operating stress.
The critical crack size ( a_c ) under the operating stress ( \sigma_o ) is given by:
We need to find a proof-test stress ( \sigma_p ) such that any crack larger than ( a_i ) will fail during the proof-test. Using the fracture toughness equation: