As for XPS results (Fig. S8a and b), the energy spectrum peaks of the 1M-5C--NML after 5…
- User
As for XPS results (Fig. S8a and b), the energy spectrum peaks of the 1M-5C--NML after 5 cycling and 100 hours of reaction show similarities with those of the original one. 换一种表述
- Assistant
Based on the XPS data provided in Supplementary Figure S8a and b, the energy spectra of the 1M-5C--NML material retain comparable peak features even after 5 cycles and 100 hours of reaction, indicating consistency with the initial material's spectral characteristics.
- User
For example, the rougher appearance due to the corrosion performances appeared in SEM images of used 1M-5C--NML. 换一种表述
- Assistant
The SEM images of the used 1M-5C--NML depict a more textured surface, which suggests that the material has undergone corrosion.
- User
For example, the rougher appearance due to the corrosion performances appeared in SEM images of used 1M-5C--NML. 换一种表述
- Assistant
The SEM images reveal that the 1M-5C--NML, after being utilized, exhibits a surface that has become coarser, indicative of the material experiencing corrosion-related degradation.
- User
For example, the rougher appearance due to the corrosion performances appeared in SEM images of used 1M-5C–NML. 换一种表述
- Assistant
The SEM images show that the surface of the used 1M-5C--NML has developed a more textured and uneven appearance, which is indicative of degradation from corrosive effects.
- User
For example, the rougher appearance due to the corrosion performances appeared in SEM images of used 1M-5C–NML. 换一种表述
- Assistant
The surface morphology of the utilized 1M-5C--NML, as observed in the SEM images, displayed increased roughness, a characteristic typically resulting from corrosion effects.
- User
For example, the rougher appearance due to the corrosion performances appeared in SEM images of used 1M-5C–NML. 用一句话转述
- Assistant
The SEM images showed that the 1M-5C--NML material had developed a rougher texture after usage, suggesting it underwent corrosion.
- User
For example, the rougher appearance due to the corrosion performances appeared in SEM images of used 1M-5C–NML. 用一句话转述
- Assistant
Post-use SEM images of the 1M-5C--NML material revealed a roughened surface indicative of corrosion.
- User
For example, the rougher appearance due to the corrosion performances appeared in SEM images of used 1M-5C–NML. 换一种表述
- Assistant
The used 1M-5C--NML exhibited a deteriorated, rough surface in the SEM images, a consequence of the corrosion it underwent.