what's the typical thickness of Pt bottom contacts?
- User
what's the typical thickness of Pt bottom contacts?
- Assistant
The typical thickness of Pt (Platinum) bottom contacts can vary depending on the specific application and requirements. However, in many cases, platinum bottom contacts are commonly in the range of 10-100 nanometers (nm) thick. Nevertheless, it is important to note that the thickness can be adjusted based on the specific needs of the device or the desired electrical and mechanical properties.
- User
When Pt bottom contacts get thicker, it will be difficult to lift off, is that true?
- Assistant
Yes, that is generally true. As the thickness of Pt bottom contacts increases, the adhesion between the Pt layer and the substrate also increases. This increased adhesion can make it more challenging to lift off the Pt layer during the fabrication process. Thicker Pt layers tend to have greater cohesive strength, making it harder to remove them without causing damage or delamination. Therefore, it is important to consider the trade-off between the desired thickness of the Pt layer and the ease of lift-off during the manufacturing process.
- User
If the AFM scan shows that the edge of the Pt bottom contacts has a bulge of about 20 nm, what may be the reason ?
- Assistant
There could be several reasons for the bulge at the edge of the Pt bottom contacts observed in an AFM scan. Here are a few possibilities:
-
Poor deposition uniformity: Uneven or non-uniform deposition of the Pt layer can lead to variations in thickness or localized bulges. This may be caused by issues with the deposition technique or parameters.
-
Interfacial stress: Differences in thermal expansion coefficients between the Pt layer and the underlying substrate can induce stress at the interface. This stress can cause the Pt layer to deform and create bulges at the edges.
-
Surface contamination: Presence of impurities, particulates, or contaminants on the surface before or during the deposition process can affect the growth and morphology of the Pt layer, resulting in bulges.
-
Surface diffusion and agglomeration: At higher deposition temperatures, surface diffusion and agglomeration of Pt atoms can occur, leading to the formation of nanoscale bulges or islands at the edges.
-
Substrate topography: If the substrate itself has an uneven or rough topography, it can influence the growth of the Pt layer and lead to localized bulges at the edges.
-
- User
What is the typical roughness of electron beam evaporated Pt ?
- Assistant
The typical roughness of electron beam evaporated Pt (Platinum) can vary depending on several factors such as deposition conditions, substrate properties, and process optimization. However, in general, electron beam evaporation can produce relatively smooth Pt films with roughness values in the range of a few nanometers (nm).
The achieved roughness can be affected by parameters such as the deposition rate, substrate temperature, deposition angle, and film thickness. By optimizing these parameters, it is possible to achieve even smoother Pt films with lower roughness values. It's worth noting that additional post-deposition treatments such as thermal annealing or surface polishing can further enhance the smoothness of the Pt film if necessary.
It is recommended to consult the specifications or technical documentation of the specific deposition system or process used to obtain more precise information about the typical roughness of Pt films achieved through electron beam evaporation.
- User
Will antimony be oxidized at room temperature?
- Assistant
Antimony (Sb) can react with oxygen in the air, leading to its oxidation even at room temperature. However, the rate of oxidation of antimony at room temperature is relatively slow. Over time, a thin layer of antimony oxide (Sb2O3) or antimony trioxide (Sb2O3) can form on the surface of antimony. This oxide layer acts as a protective barrier, preventing further oxidation of the underlying antimony metal.
It's important to note that the rate of oxidation can be influenced by factors such as humidity, presence of other reactive substances, and surface conditions. In environments with high humidity or elevated temperatures, the oxidation rate of antimony can be accelerated. Additionally, impurities or contaminants on the surface of antimony can facilitate oxidation reactions.
To minimize oxidation, antimony can be protected by storing it in a controlled environment with low humidity or through the use of protective coatings.