Below is a paragraph from an academic paper. Polish the writing to meet the academic style, improve the spelling, grammar, clarity, concision and overall readability. When necessary, rewrite the whole sentence. Furthermore, list all modification and explain the reasons to do so in markdown table. Paragraph: To investigate the effect of SiO2 addition on the glass content of the slag, municipal solid waste incineration fly ash was mixed with 10%, 15%, 20%, and 30% SiO2, respectively. The mixture was subjected to thermal treatment at 1400 °C and subsequently quenched with water. The resulting thermal treatment products were dried, ground, and characterized. The XRD spectra of the thermal treatment products of the municipal solid waste incineration fly ash with different amounts of SiO2 added are shown in Figure 19. It can be observed that the mineral Ca(OH)2 exists in the thermal treatment products at 1400 °C, possibly formed by the reaction of the quenched slag with water due to the reaction of CaO with water. Through the addition of SiO2, calcium silicate (Ca2SiO4), the original calcium oxide in the municipal solid waste incineration fly ash, is formed through a reaction. With the increasing amount of SiO2 added, the formation of an amorphous non-crystalline structure gradually occurs. By analyzing the XRD spectra, the glass content of the thermal treatment products of the municipal solid waste incineration fly ash with different amounts of SiO2 added can be obtained, as shown in Figure 20. It can be observed that the addition of SiO2 promotes the formation of glassy materials during the incineration fly ash melting process, leading to an increased proportion of heavy metals transferred into the dense glassy structure. Furthermore, the glass content of the thermal treatment products increases with the increasing amount of SiO2 added, enhancing the stability of the slag to a certain extent.
- Assistant
- User
Due to the high proportion of amorphous composition in the products obtained from high-temperature melting and thermal treatment, X-ray diffractometers cannot provide composition information about amorphous materials. In contrast, infrared spectroscopy is highly effective in studying the composition and structure of minerals. It is particularly useful in revealing short-range ordering between atoms, and the absorption peak positions in infrared spectra can be used for qualitative analysis of structural groups [18,19]. Therefore, in this section, infrared absorption peaks are used for structural characterization of the thermal treatment products in order to investigate the influence of different SiO2 addition ratios on the network structure of the products. Since the infrared vibrational absorption spectra region that reflects the composition and structure of the thermal treatment products is generally fixed, the wavenumber range from 400 to 1600 cm-1 was selected. Figure 21 shows the infrared absorption peaks of the thermal treatment products of municipal solid waste incineration fly ash with different amounts of SiO2 added, processed at 1400 °C.
- Assistant
- User
SiO2 belongs to the network-forming agents and serves as the basic structural unit in building the glass network, playing a role in the skeleton of the ash network. According to previous literature reports [20-22], the vibrational origins of these infrared absorption peaks are generally consistent. The positions and characteristic peaks of the infrared spectrum vibrations are shown in Table 4.
- Assistant
SiO2 is classified as a network-forming agent, acting as the fundamental structural component in constructing the glass network and contributing to the framework of the ash network. Consistent with previous literature [20-22], the vibrational origins of these infrared absorption peaks remain generally uniform. Table 4 presents the positions and characteristic peaks of the infrared spectrum vibrations.
Modifications:
- Replaced "serves as the basic structural unit in building the glass network, playing a role in the skeleton of the ash network" with "acting as the fundamental structural component in constructing the glass network and contributing to the framework of the ash network" - To improve clarity and use more concise language.
- Added "Remains" before "generally consistent" - To provide continuity with the previous sentence and improve readability.
- Replaced "The positions and characteristic peaks of the infrared spectrum vibrations" with "Table 4 presents the positions and characteristic peaks of the infrared spectrum vibrations" - To improve clarity and specify where the information can be found.
- User
From Figure 21, it can be observed that at 1400 °C, with an increasing amount of SiO2 added, the absorption peaks in the range of 670-800 cm-1 and 800-1200 cm-1 tend to gradually shift towards higher wavenumber ranges. This indicates an increase in the frequencies of the absorption peaks associated with the Si-O-T (T=Si/Al) network structure in the thermal treatment products. It suggests an increase in the content of [SiO4] units, which enhances the connectivity of the ash network structure. As a result, the silicate chains grow, leading to an increased degree of network aggregation in the thermal treatment products. The addition of SiO2 provides Si4+ ions that form [SiO4] tetrahedra, thereby enhancing the network connectivity of the Si-O framework. Based on the above findings, the following conclusions can be drawn: increasing the SiO2 content promotes the formation of [SiO4] and Si-O-T (T=Si/Al) structures, resulting in a denser structure of the thermal treatment products. This increased densification poses challenges for rearrangement processes, thereby increasing the tendency of the thermal treatment products to vitrify and increasing the glass content.
- Assistant
- User
To investigate the influence of heat treatment temperature on the formation of glassy phase in fly ash with the addition of SiO2, 20% SiO2 was added to the municipal solid waste (MSW) incineration fly ash, resulting in a Si/Ca ratio of 0.751. The fly ash samples were then subjected to heat treatment at temperatures of 1100, 1200, 1300, and 1400 °C, followed by water quenching. Subsequently, the heat-treated products were dried, ground, and characterized, and the obtained X-ray diffraction (XRD) patterns are shown in Figure 22. It can be observed that with increasing temperature, the transformation of minerals in the fly ash occurred, leading to a reduction in the types and content of minerals, while the amount of amorphous glassy phase increased. At 1100 °C, the main crystalline phases in the fly ash were NaCl, anhydrite (CaSO4), gehlenite (Ca2MgSi2O7), larnite (Ca3Si2O7), and merwinite (Ca3MgSi2O8). As the temperature increased to 1200 °C, NaCl gradually volatilized at high temperature, and CaSO4 decomposed to form CaO, which subsequently reacted with SiO2 to form silicates. At 1300 °C, the fly ash underwent transformations and generated Ca2SiO4, while at 1400 °C, the XRD pattern of the heat-treated product exhibited a “bread-loaf” peak, indicating the presence of glassy phase. By analyzing the XRD patterns, the glassy phase content in the heat-treated products of the MSW incineration fly ash with 20% SiO2 addition was obtained, as shown in Figure 23. It can be observed that the content of glassy phase in the heat-treated products increased with the rise in temperature. From a thermodynamic perspective, as the temperature of a crystalline material increases, its entropy increases, leading to an increase in disorder within the structure, favoring the formation of glassy phase. The results indicate that with increasing heat treatment temperature, the content of glassy phase in the heat-treated samples increased. Therefore, the heat treatment temperature plays a crucial role in the formation of glassy phase.
- Assistant
To investigate the impact of heat treatment temperature on the formation of the glassy phase in SiO2-added fly ash, 20% SiO2 was incorporated into municipal solid waste (MSW) incineration fly ash, resulting in a Si/Ca ratio of 0.751. Subsequently, the fly ash samples underwent heat treatment at temperatures of 1100, 1200,