Translation: The isomerization of low-carbon alkanes is an important technology for optimizing the composition of gasoline pools in China. The key to this technological innovation lies in the development of efficient catalysts. Nickel, due to its excellent hydrogenation/dehydrogenation activity, low cost, resistance to poisoning, and abundant reserves, has become a highly promising metal for the development of dehydroisomerization catalysts. However, its relatively lower hydrogenation and dehydrogenation activities compared to noble metals require a significantly higher loading amount, which poses a serious challenge to its dispersion. Therefore, increasing the dispersion of the metal component is crucial for the development of efficient non-noble metal dehydroisomerization catalysts. However, the construction of Ni nanoclusters for low-carbon alkane dehydroisomerization and their surface effects have been rarely explored to date. In this thesis, with the aim of developing efficient catalysts for low-carbon alkane dehydroisomerization, the method of constructing highly dispersed Ni on the surface of SAPO-11 molecular sieves was established, and the mechanism of improving Ni dispersion and the effect of sub-nanometer-scale Ni-induced surface effects were investigated, in order to provide a theoretical basis for the development of efficient Ni-based catalysts for low-carbon alkane dehydroisomerization.
Ni/SAPO-11 catalysts with adjustable Ni particle sizes were prepared using an ionic liquid-assisted method. It was found that the ionic liquid [Bmim][BF4] can form coordination compounds with Ni2+, and the steric hindrance effect of the ligand effectively inhibits the aggregation and growth of Ni. By varying the amount of the ionic liquid, the particle size of Ni can be effectively controlled, reducing the average particle size from 19.9 nm without the addition of the ionic liquid to 7.2 nm. Furthermore, using nickel acetylacetonate as the precursor for Ni further improved the dispersion, reducing the particle size to 5.3 nm. To investigate the influence of the geometric properties of Ni clusters on the isomerization performance of the catalyst, the turnover frequency (TOF) values of catalysts with different Ni particle sizes were calculated, and the results were correlated with DFT simulation results to investigate the influence of Ni atoms at different positions in the catalyst on the dehydrogenation performance of n-hexane. The results showed that the TOF of the catalyst with an average metal particle size of 5.3 nm was twice that of the catalyst with a size of 11.7 nm. DFT calculations further revealed that the activation energies required for the dehydrogenation of n-hexane on the platform Ni sites were 1.1 and 1.6 times higher than those on the edge and corner Ni sites, respectively, which is consistent with the evaluation results of the catalysts, indicating that the catalyst with the highest Ni atom proportion on the edge and corner sites has the highest intrinsic catalytic activity for the isomerization reaction.
To further reduce the particle size of Ni clusters on the SAPO-11 surface, a dual-ligand co-assisted method was used to suppress the aggregation of the nanoscale Ni clusters during the calcination and reduction processes. Since the aggregation of metal particles often occurs during the calcination and reduction processes of catalysts, this study coupling the geometric effects of Ni2+ migration induced by the lysine ligand during the calcination process with the inhibitory effect of the ionic liquid on Ni migration during the reduction process, effectively suppressed the aggregation and growth of Ni species throughout the process. The interaction modes and energy barriers between lysine and Ni2+ ions, as well as between the ionic liquid and Ni clusters, were calculated using density functional theory (DFT). The results showed that lysine and Ni2+ can form stable tetrahedral compounds, which help to inhibit the aggregation and growth of nickel oxide during calcination. Introducing the ionic liquid during the reduction process significantly increased the energy barrier for the formation of Ni clusters, from 0.38 eV without the addition of the ionic liquid to 1.15 eV, with the anion playing a dominant role in stabilizing the Ni clusters and regulating their electronic structure. Guided by DFT calculations, a method for co-assisted preparation of highly dispersed nickel-based catalysts using the ionic liquid and lysine was established. Transmission electron microscopy (TEM) showed that the combined action of lysine and the ionic liquid promoted the high dispersion of Ni, resulting in ultra-small Ni particles with an average size of 4.4 nm. At the same time, the introduction of the ionic liquid during the reduction process increased the electron cloud density of Ni, which is beneficial for the activation and desorption of H species on the Ni active sites. These factors together promoted the timely conversion of reactants and intermediate products. The obtained catalysts exhibited significantly better performance in n-hexane dehydroisomerization compared to Ni/SAPO-11 catalysts prepared by traditional impregnation methods, with a maximum isohexane yield of 67.2% and a TOF of 16.5 h-1, which is 2.3 times and 2.8 times higher, respectively.
The preparation method is an important approach to control the particle size of the metal component. In this study, an in situ sol-gel method assisted by ligands was successfully used to prepare sub-nanometer Ni clusters in the SAPO-11 catalysts, and the geometric and electronic effects of sub-nanometer Ni clusters were systematically explored. It was found that the proportion of edge and corner Ni atoms in sub-nanometer Ni clusters was as high as 85%, far exceeding that in nanoscale Ni clusters. Characterization results such as H2-TPD and FTIR showed that the sub-nanometer Ni clusters exhibited stronger adsorption/activation abilities for C-H and H-H bonds due to their abundant dangling bonds and high surface energy. To further reveal the underlying reasons for the influence of the surface effects of sub-nanometer Ni clusters on the adsorption/activation of reactant molecules, the partial density of states (PDOS) and the orbital center variations of Ni clusters with different particle sizes were calculated using DFT simulations. The results revealed that the reduction in particle size to the sub-nanometer scale was accompanied by an increase in the center of the d-band and a decrease in the occupancy of anti-bonding orbitals, which is conducive to enhancing the interaction between Ni active sites and reactants, thereby improving the adsorption and activation capabilities of sub-nanometer Ni clusters for C-H and H-H bonds. Reaction results showed that the sub-nanometer Ni clusters in the Ni/SAPO-11 catalyst exhibited superior catalytic activity in n-hexane hydrogenation isomerization compared to the nanoscale Ni clusters of Ni/SAPO-11. The catalyst with sub-nanometer Ni clusters achieved a maximum isohexane yield of 67.2% and a TOF of 16.5 h-1, which were 2.3 times and 2.8 times higher, respectively, than those of the catalyst with nanoscale Ni clusters.